Fab & Assembly Experts, I am seeing some kind of contamination to bare boards. I have put pictures at Steve web site for everyone's review and here is the link. http://www.stevezeva.homestead.com <http://www.stevezeva.homestead.com/> Does anyone have seen similar kind of contamination? Is it some kind of corrosion? It looks outside of board to me but not sure as I have seen the boards personally yet. Boards are processed Electroless Nickel Immersion Gold. Any help will be highly appreciated. Re, Ken Patel --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------