Has anyone experienced poor conformal coat wetting due to moisture on the pwb surface? Could moisture embedded in the pwb be problematic? In our process, we batch clean our boards which includes multiple deionized water rinse cycles. The product is then baked at 250°F for 2 hours. We have a new solder mask material which coats well prior to our processing. The 2 hour bake at 250°F has always proved adequate. Is anyone using a longer bake time? What is the substantiation for establishing an extended time? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------