I made a very stupid typo, giving me nothing but unusefull answers: I meant to write IPC4101/26, not 4104/26. Seems I didn't have enough coffee this morning. Sorry.... Daan >>> [log in to unmask] 10/05/04 12:27pm >>> Daan, IPC4104 is the HDI material spec and I didn't think there was a /26 material in it, and unless it's been updated since I last looked I don't remember there being glass reinforced materials in it at all. Regards Ian Fox Goodrich ECS -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Daan Terstegge Sent: 05 October 2004 10:45 To: [log in to unmask] Subject: [TN] Laminate per IPC-4104/26 Hi Technet, I need to make a quotation for a boardassembly with laminate and prepreg per IPC-4104/26. I don't have the spec available, nor could I find something with Google. Does anyone know what kind of material this is ? Daan Terstegge Thales Land&Joint Systems Unclassified mail Personal Website: http://www.smtinfo.net --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------