Jenning's original paper cites the conditions of dendrite formation as going from 'cathode to anode'. When I visited him at his Sandia Lab, he just called them dendrites which grew from cathode to anode, the CAF designator came later. Bill Kenyon Global Centre Consulting 3336 Birmingham Drive Fort Collins, CO 80526 Tel: 970.207.9586 New Cell: 970.980.6373 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------