Are the coupons scaled the same as the images? Are you sure? Is it a sequential lamination? If the drill is scaled (even from the center) it still has to be positioned relative to the innerlayer images correctly. How is this done? Are you using a drill optimizer (Smart Drill, Pluritec or the like)? If so, where are the optimizer targets? Tim Reeves Process Engineer Tyco Electronics | Printed Circuit Group | Dallas Division 1270 Monmouth Cutoff Road, Dallas, OR 97338 503.623.1000 Ext.1120 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Tuan Le Sent: Thursday, October 07, 2004 10:53 AM Subject: Registration problem Hello Technetters, Lately I have been having this problem with some rigid-flex panels: X-ray after drill shows good registration on coupons (which are located at each corner and along the edges) but bad registration inside the panels (from small annular rings to breakouts). * Everything on a layer is scaled from the center of the layer. * Layer to layer registration is good. Inside the panel, however, registration is good on the lower left corner but starts getting bad towards the right and top of the panel making it look like drill is scaled from the lower left corner. Drill operator confirms that drill is scaled from the center not the corner. I can't explain how this problem happened and would appreciate any help. Thank you in advance. Tuan Le --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------