Steve, Was the crack merely cosmetic or is there potential for wire damage with the excess potting compound? Jim Carlson Reliability/Quality Engineer Rockwell Collins Steve Gregory <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 10/29/2004 05:04 PM Please respond to TechNet E-Mail Forum; Please respond to SteveZeva To: [log in to unmask] cc: Subject: [TN] Cracked Cases on SMT Power Inductors from Coil Craft... Hi All! I just discovered a problem with some SMT Coil Craft Power Inductors, it's their MSS1260 series. The problem is that the cases are cracking. I don't know if any of you have experienced this, or know anything about this issue, so I thought I would share what I just learned this afternoon. Take a look at: http://www.stevezeva.homestead.com/files/CrackedCoil.jpg We just discovered these on assembled product..naturally :^( I called Coil Craft and spoke with their Quality representative, and they said that they are aware of the issue, and have changed their assembly processes back on September 16th to address the issue. The reason that the coil cases were cracking, was because they were filling the entire cavity between the surface of the winding around the coil, and the inside surface of the case with potting compound. During subsequent heating, the expansion of the potting compound would stress the case and cause it to crack. I was told that inductors made after September 16th would only have potting compound in the corners to allow for expansion. So if any of you have any of these sitting around in your stockroom, I wouldn't use them without inspecting them to see if the cavity is completely full of potting compound. -Steve Gregory- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------