Robert If you need this info to run cleanliness test - urghh I hate that expression - then as a ROT (Rule Of Thumb) take the square of the board and multiply by 3 - that's both sides plus an allowance for the componentry. Don't forget you have the surface top AND bottom to account for.... If you are out it will almost certainly be on the low side, and for Ionic Contamination Testing (there, now I feel better) this might be a good thing not a bad thing. What do I mean? Well, if the surface area is lower than reality, then the result will suggest that there is more contamination per square than there might be, which in turn means you might improve your cleaning operation to get the desired result and that cannot be a bad thing - surely? (Empty Mountain Dew Cans incoming?) -- Regards Graham Naisbitt [log in to unmask] Concoat Limited - Engineering Reliability in Electronics A British Manufacturer www.conformalcoating.com www.concoat.co.uk www.concoatsystems.com Golf Quote of the week: Every time I try to tell myself this is going to be fun today. I try to put myself in a great frame of mind before I go out - then screw it up with the first shot! Cell: 079 6858 2121 Office: +44 (0)1252 813706 > Hi T'netters; > Is anyone aware of a program that calculates the surface area of > components so I can more accurately determine the surface area of PCB > assemblies? > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for > additional information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ----------------------------------------------------- > Thanks in advance. > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------