Conductive is less than 10^5 ohms per square. Dissipative is between 10^5 and 10^12 ohm square, or volume resistance between 10^4 and 10^11 ohms-cm . Greater than 10^12 ohms per square or volume resistance 10^11 ohm-cm is insulative. check: http://www.kodak.com/global/plugins/acrobat/en/digital/ccd/applicationNotes/electrostaticDischarge.pdf Regards, Ramon -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Blair K. Hogg Sent: Wednesday, September 22, 2004 11:49 AM To: [log in to unmask] Subject: Re: [TN] ESD FLOOR Is the conductivity of the floor in ohms / sq cm known? That would help determine whether it is hazardous given electrical equipment is present. IMHO, the difference between dissipative and conductive is semantics, but perhaps there is a range for each, e.g. dissipative is > 10k per sq cm and conductive is between 100 and 10k ohms per square cm. >>> [log in to unmask] 09/21/04 09:54AM >>> Hello Technet, a quick question... For a clean room application (microelectronics assembly), which is more appropriate, a conductive floor or a dissipative floor (and why)? ******************************************************************* This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the system manager. This footnote also confirms that this email message has been swept for the presence of computer viruses. www.hubbell.com - Hubbell Incorporated --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------