hi, i believe you should be able to use a gasket material such as viton. phil -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Douglas O. Pauls Sent: Monday, August 16, 2004 2:02 PM To: [log in to unmask] Subject: [TN] thin film Good day all, I am in need of a recommendation for a thin film sealant material. I need it to be 15-20 mils thick, cuttable, and preferrably non silicone. We have considered the Sil-Pad technology, but as this will be used in a vacuum seal operation, I am concerned about silicone outgassing or cross contamination. Are there any thin gasket materials from the engineered rubbers that anyone would recommend? Doug Pauls --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------