Hi Dave, You may wish to try wirebondable soft gold plating. It has higher purity,different crystal structure, deposit properties. Hard gold much more loaded with organics and metallic brighteners (Ni or Co) and normally better suits for high wear resistance. Aleks Lozinsky Technic Toronto ----- Original Message ----- From: "R Sedlak" <[log in to unmask]> To: <[log in to unmask]> Sent: Wednesday, August 11, 2004 8:50 PM Subject: Re: [TN] SOFT Gold Plating/Contaminate Question Dave: The purpose of plating brighteners is to co-deposit, and muck up (a technical term, meaning to "muck-up") the chrystalline deposit, and make it shiney. And if you get too many, or you get some brightener breakdown problems, which does occur a lot in gold plating, because of the inert anodes, you can get excessive organics in your gold. And the type of structures you are seeing are exactly what you would expect... See, contrary to the common wisdom, electroplating does (sometimes) follow the rules of chemistry. Rudy Sedlak "David D. Hillman" <[log in to unmask]> wrote: Hi TechNet! Hey, looking for some help (Rudy, Frank, Gerard, plating folks). Background: I have a test board which with approximately 80 uinches of wirebondable hard gold plating that is having gold wirebond process problems. An XPS (xray photoelectron spectroscopy) analysis of a "good" versus "bad" test board revealed that the "bad" has significant organic surface contamination for carbon and oxygen in the form of a hydrocarbon (lots of C-C and C-H bonds). Now the question: can/will a hydrocarbon species be codeposited into the gold plating thickness? I understand the surface process/issues but the codeposit question came up. Dave Hillman Rockwell Collins [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- __________________________________________________ Do You Yahoo!? Tired of spam? Yahoo! Mail has the best spam protection around --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- http://mail.yahoo.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------