1. Number of preheaters on wave - 3, convection, IR and quartz heaters 2. Typical conveyor speed - 0.8 to 1 m / min 3. Typical topside/bottomside preheat temp 110 to 130 deg c 4. Do you wave solder SOIC or other components besides chips? - yes Cheryl Tulkoff <cheryl.tulkoff@ To: [log in to unmask] NI.COM> cc: Sent by: TechNet Subject: [TN] Anyone using VOC-free wave solder flux? <[log in to unmask] > 16/08/2004 15:42 Please respond to TechNet E-Mail Forum; Please respond to Cheryl Tulkoff Is anyone out there using a VOC-free (water-based) wave solder flux? I'm looking for users who would be willing to share some information with me like the following: 1. Number of preheaters on wave 2. Typical conveyor speed 3. Typical topside/bottomside preheat temp 4. Do you wave solder SOIC or other components besides chips? Thanks, Cheryl --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------