Deborah, You are right, the current version is issue 1, from Sept. 1997. Bellcore/Telcordia has lost a lot or their experts and have gone to following more of the industry standards. They do however still require this specification be met. Russell Nowland Lucent Technologies Quail Springs Parkway Plaza 14000 Quail Springs Parkway. Suite 300 Oklahoma City, OK 73134 Phone: 405-302-1660 Fax: 405-302-1622 Cell: 405-203-0034 email: [log in to unmask] -----Original Message----- From: Deborah Schepis [mailto:[log in to unmask]] Sent: Friday, July 30, 2004 3:10 PM To: [log in to unmask] Subject: [TN] Bellcore / Telecordia A Friday afternoon question... Does anyone know what the most recent version of the Bellcore / Telecordia spec is? The latest I have is the GR-78-CORE which is dated 1997. Is that it? If not, where can I find the most recent version? Thanks, Debbie Deborah S. Schepis Quality Engineer Endicott Interconnect Technologies (607) 755-3152 email: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------