Tote trays are readily available in stock sizes from several manufacturers. For electronics, you probably want ESD safe trays. I recommend the black conductive trays for clean room use, as the antistatic coating on the blue static-dissipative trays washes off when you clean them to go into the clean room. The black conductive trays have carbon particles molded into the plastic, so they won't wash off. I used to work for a disk drive repair facility where we discovered the problem with the blue dissipative totes. McMaster-Carr (www.mcmaster.com) and various other distributors sell conductive trays in several sizes. Matching dividers are available, too. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly Sent: Wednesday, August 25, 2004 9:21 AM To: [log in to unmask] Subject: [TN] Plastic tote trays Good morning, We are looking for sources for tote trays to carry flex materials through our plant especially in the clean room areas. any suggestions would be helpful. Thanks. Steve Kelly PFC Flexible Circuits Limited Ph: (416) 750-8433 Fax: (416) 750-0016 Cell: (416) 577-8433 E-Mail: [log in to unmask] _____ <http://promos.hotbar.com/promos/promodll.dll?RunPromo&El=&SG=&RAND=38685&pa rtner=fastutility> Block Spam Emails - Click here! --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------