I remember a general rule of 20-25% larger for wave. Smaller pin sizes need to be tighter - much depends on the insertion capability and component type. Jeffrey Bush Director, Quality Assurance and Technical Support 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302-1890 Tel. 802.257.4571.21 Fax. 802.257.0011 [log in to unmask] http://www.vtcircuits.com -----Original Message----- From: Pasquito, Helena [mailto:[log in to unmask]] Sent: Monday, July 12, 2004 12:39 PM To: [log in to unmask] Subject: [TN] Pin Size vs. Plated Through Hole Size I am looking for a specification that would have information on 'pin size' vs. 'plated through hole size' design requirements/recommendations/limits for wave soldering applications. Does anyone know of any such specification (internal or external)? Thank you for any help you can offer. Helena Pasquito Quality Training Admin./CRM Tyco Electronics M/A-COM 1011 Pawtucket Blvd. M/S150 Lowell, MA 01853 Phone 978-442-5024 Email [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------