I would use IPC-6012 as a reference - the finishes and abb. are specified there. Tin, Silver and OSP do not have a min/max thickness, while ENIG and electrolytic finishes should have a thickness specified. ENIG - EN is generally 100 uinch min and IG is 2-10 uinches. Jeffrey Bush Director, Quality Assurance and Technical Support 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302-1890 Tel. 802.257.4571.21 Fax. 802.257.0011 [log in to unmask] http://www.vtcircuits.com -----Original Message----- From: Kane, Joseph E [mailto:[log in to unmask]] Sent: Thursday, July 01, 2004 5:04 PM To: [log in to unmask] Subject: [TN] Specifying PWB Finishes We're preparing to order some test boards with alternative finishes for lead-free testing, including immersion tin and OSP over bare copper. Can anyone suggest how we might specify these board finishes in a drawing note? Our existing drawings pretty much specify only the material and the thickness, something like "immersion gold, xxx thick, over electroless nickel, xxx thick." Joe Kane BAE SYSTEMS Controls Johnson City, NY --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------