Siggi: I'm not sure why you can't use a 2 component glue. "long stick time" are you saying that the cure time is too long? If that's the case there are many fast set, 2 part epoxies that will bond very well to a PCB and/or soldermask substrate. These will cure in less than 5 mins at 23C. There are some that will cure even faster but the adhesive mass must remain small to prevent excessive exotherm. Loctite, CIBA, 3M, etc, all make a variety of these fast curing 2 part epoxy structural adhesives. Regards Michael Barmuta Staff Engineer Fluke Corp. Everett WA 425-446-6076 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Zweigart, Siegmund Sent: Friday, July 02, 2004 8:29 AM To: [log in to unmask] Subject: [TN] Glue on PCB Hello all I have to Glue some guidepins to a PCBA. Can anybody give some inputs which glue is possible? I think cyano based glues are not possible on soldermask / PCBA. 2 component glue are no option due to long stick time. Any recommendations? Best regards Siggi --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------