Green or yellow is all I am aware of that can be flexed. Good luck. Steve Kelly -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Roger Tingler Sent: Wednesday, June 16, 2004 9:00 AM To: [log in to unmask] Subject: [TN] White LPI Flex soldermask GOOD MORNING, Fellowtechnetters Does anyone know of a white LPI (Liquid Photo Image able) Solder mask that can be used for Flex circuit boards? The flex is extremely dense and will bend only once to a generous cone shape. Unfortunately, the typical LPI used for our rigid boards will crack. THANKS in advance for your support, Roger --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------