Just wanted to test my e-mail setup for this newsgroup. Please Delete. Thanks TDK -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Graham Naisbitt Sent: June 10, 2004 3:59 AM To: [log in to unmask] Subject: Re: [TN] Conformal Coating Importance: High Lance Are you sure this is happening on the leads of the components? If the answer remains yes, then this would worry me. The problem is de-wetting. The cause of which is often attributed to silicone contamination from mould release agents, masking residues, staking compounds or maybe adhesive residues. It is also conceivable that it is present in the feed lines of a spray gun or nozzle, especially if it has been used to apply a silicone coating for another application. I assume that you are inspecting this under UV (Black) light? If so, then please verify that you can observe this happening by coating under the light source. If it is, then I am confident this is a silicone issue. Otherwise, is this problem appearing on the vertical or horizontal surfaces? If you can, maybe you could take a photo and post it to Steve's web site, then we could all take a look - a picture is often worth a thousand words...and therefore a darned site quicker! Graham Naisbitt > Hello again Techies; > > We are having issues with our conformal coating on some of our components. > It pulls back from some of the components leads along the edges. > We are wondering if this will make a difference in the protection of the > board. > We're using Humiseal Acrylic 1B31 and Humiseal Thinner 521 in a mixture. > The conformal machine sprays a nice coating and then the coating starts to > recede. Sometimes this happens even when we paint the acrylic manually. > Has anyone else ran into this problem, and what to do to overcome it? > > This is a good one for the end of the day. I'll be waiting. > > Thanks again > > > P. Lance Mayes > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for > additional information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ----------------------------------------------------- > Mfg. Trainer > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------