It is important to know the warpage/camber/coplanarity in the BGA attach site on reflow cool down as you pass through the freeze point of the solder. If the PCB stack up is poorly balanced, or a heavy Cu plane terminates half-way under a BGA attach site, or board lamination conditions (pressure, typically) across a large BGA site is not uniform, a BGA site may be coplanar at room temp and be badly warped at the freeze point. Leo ------------------------------------ Leo M. Higgins III, Ph.D. Director of Applications Engineering / ASAT Inc. [log in to unmask] 3755 Capital of Texas Hwy-So Suite 100 Austin, TX USA 78726 tel: 512-383-4593 fax: 512-383-1590 mobile: 512-423-2002 ------------------------------------ -----Original Message----- From: Lum Wee Mei [mailto:[log in to unmask]] Sent: Tuesday, June 08, 2004 7:03 PM To: [log in to unmask] Subject: Re: [TN] Flex Rigid PCB Surface Coplanarity Philip, I am no reliability gal. However, from what I have been asking around some time back regarding coplanrity especially for BGA, the board bow & twist formula and technique is applicable. Instead of taking the entire board, you should concentrate on the BGA footprint area. This BGA area now become your board. Find the reading around this area as you would for board. For PTH, bow & twist <1%, SMT <0.75% and for BGA <0.5%. Do not asked me how the 0.5% comes about, it would given to me by Dr John Lau when I asked about this bow & twist for BGA. I guess it has something to do with the solder ball coplanarity being 6 mil. That's is all I can share. Hope it is of some help. Regards, Wee Mei Anslow, Phillip wrote: >Dear TechNetters, > >Please can anyone point me to any specification covering the coplanarity of >the footprints on the PCB surface? > >I've looked in IPC-A-600F and IPC-6010 series, and, whilst flatness in terms >of bow and twist is specified, there does not appear to be anything >regarding the coplanarity across a component footprint. I have a current >design where the use of thin dielectrics fear may tend to ape the copper >topography on the underlying layers (they are predominantly tracks rather >than planes). The footprints happen to be BGA, CGA and QFP for ceramic >packages and whilst I have not yet received the boards they are to be >assembled to, I would like to be aware if I should do measurements and to >what limits are acceptable on receipt. I am concerned excessive undulation >may give some soldering issues with opens but don't know if my concerns are >unfounded. > >I believe various studies and consortia have measured surface coplanarity in >the past during studies into soldering processes etc, but unfortunately I >lost touch with the conclusions due to an outsourcing strategy of a big OEM. >Maybe these concluded that board coplanarity is not an issue but if anyone >can help reassure me, particularly regarding flex rigid PCBs with thin >dielectrics, or if anyone has previous experience in this area you could >share, I'd be very grateful. > >Many thanks in advance. > >Phil Anslow. > > >******************************************************************** >This email and any attachments are confidential to the intended >recipient and may also be privileged. If you are not the intended >recipient please delete it from your system and notify the sender. >You should not copy it or use it for any purpose nor disclose or >distribute its contents to any other person. >******************************************************************** > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 >----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------