Craig, Although Immersion Silver is a good choice for a lot of reasons, it would be the last choice compared to all the others for applications dealing with press-fit or compliant pins(IMHO). Dewey -----Original Message----- From: Craig Cullum [mailto:[log in to unmask]] Sent: Wednesday, June 09, 2004 6:27 AM To: [log in to unmask] Subject: [TN] Immersion Silver finish and press-fit connectors Hello all, We are considering switching from HASL to Immersion Silver finsih on our PCBs. How would this impact the 2mm press-fit connectors? Anyone willing to share their experiences? Thank you in advance. Regards, Craig Craig Cullum, Engineering Technologist, AMTELCO e: [log in to unmask] [log in to unmask] f: 608 838 8367 v: 608 838 4194, or 4197, x128 Visit AMTELCO at www.amtelco.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------