Hello all- Thanks for the valuable input. In regards to no clean cleaning is a process decision. We do paste/ paste on double sided boards. For the through hole components we run them through the wave soldering machine. We use a selective soldering pallet to do the through hole components. Our Wave fluxer is a foam style. When we flux the boards the excess flux gets trapped under the selective soldering pallet and never burns off . This excess flux, schmootz, gooo, famunda, spooge is left behind and is pretty thick. OK why don't we Glue/paste? is the dozens of resistor networks that populate the board bottom. I hope this makes sense. Cal -----Original Message----- From: Susan Mansilla [mailto:[log in to unmask]] Sent: Thursday, June 17, 2004 2:37 PM To: [log in to unmask] Subject: Re: [TN] Cleaning PCB's With Ultrasonics... The first item in your process is NO CLEAN. What testing has someone done to determine the need for this extreme cleaning of assemblies using no clean processes? Susan Mansilla Robisan Lab --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------