Guenter, You think we don't need higher temperature profile for running mixed components (lead and lead-free) using eutectic solder at assembly house? Re, Ken Patel -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Guenter Grossmann Sent: Wednesday, June 02, 2004 12:03 AM To: [log in to unmask] Subject: [TN] Antw: [TN] Impact of Mixed, Lead and Lead-free,components on assembly proce sses Ken (1) No as long as you avoid Bi (2) No (3) Higher temperatures are only necessary if you use lead free solder (4) Component manufacturers are changing their components now to be used for lead free solder and hopefully will let you know. However, if you intend to switch to lead free it is wise to start asking your supplier now about a roadmap. (5) European companies are starting now (and not too early). Many are at the stage where they produce first pilot lots with lead free solder. Best regards Guenter EMPA Swiss Federal Laboratories for Materials Testing and Research Centre for Reliability Guenter Grossmann, Senior Engineer 8600 Duebendorf Switzerland Phone: xx41 1 823 4279 Fax : xx41 1 823 4054 mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------