ICP probably is one of the best choices. Surface analysis (EDS, SIMS or any other) won't do it. Vladimir Igoshev, Research in Motion 451 Phillip St. Waterloo, ON, N2L 3X2 Voice: (+1) 519-888-7465, ext. 5283 Fax: (+1) 519-886-0863 E-mail: [log in to unmask] -----Original Message----- From: David Harman [mailto:[log in to unmask]] Sent: Thursday, May 27, 2004 5:00 PM To: [log in to unmask] Subject: Re: [TN] Lab You might try Rega analytical in Santa clara off Scott. I know they can do SEM and surface measurements, however I am not sure of the capability. David Harman -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stolar, Paul W Sent: Thursday, May 27, 2004 1:49 PM To: [log in to unmask] Subject: [TN] Lab Does anyone know of an analytical lab where they can do analysis of solder down to %0.1 ? XRF should work, but I am not picky. Paul Stolar Materials/Reliability Engineer Manufacturing Reliability Lead Engineer Baker Atlas 713-625-5376 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------