Hi Doug, Section 5.1 of MIL-HDBK-2000 is devoted to soldering irons and the required tests per MIL-STD-2000. The content is several pages concerning compliance tests for voltage, resistance to grd. and temperature control. Several testers were available and commonly used to automate this process. They were produced by the iron manufacturers or independent testing resources. Not knowing the iron type you may have, the manufacturer may be a good source. Lessons learned in the process of testing irons under 2000 are reflected in Revision A to MIL-STD-2000, which removed temperature testing other than regulation capability for temperature controlled soldering irons. I can send you copies of the references if you don't have them available. Best regards, Mel Mel Parrish 256 705 5530 [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Doug Sent: Friday, May 21, 2004 2:02 PM To: [log in to unmask] Subject: [TN] Solder Iron Tip Temperature & Calibration What is the accepted procedure to "calibrate" the solder iron tip temperature to MIL-STD-2000, +/-10 degrees of the selected temperature? I would not expect the digital readout to match the solder iron tip as measured using a "thermocoupled solder bead sensor" due to the expected heat loss. Must I use an embedded thermocouple into a tip? Is the digital readout required to match the tip temperature? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------