IPC4101 replaced MIL-P-13949... material spec for glass/epoxy boards. Bill Brooks PCB Design Engineer , C.I.D., C.I.I. Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 http://pcbwizards.com -----Original Message----- From: Steve Gregory [mailto:[log in to unmask]] Sent: Thursday, May 20, 2004 2:30 PM To: [log in to unmask] Subject: [TN] MIL-P-39949?? Afternoon All! We have a fab drawing here that has a note that the laminate can be either GFG or GFN, but must comply with MIL-P-39949...what is MIL-P-39949?? I've looked and looked, at DSCC and everywhere, but can't find anything on the above spec. Anybody know what that is? Thanks! -Steve Gregory- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------