The surface copper thickness shall not be less than 20% of the finished minimum requirement. This is basically for foil tolerance and processing tolerances. IPC-6012 Class 2 and 3. Section 3.5 is conductor definition. Watch for impedance requirements, this could affect the resulting performance. Jeffrey Bush Director, Quality Assurance and Technical Support 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302-1890 Tel. 802.257.4571.21 Fax. 802.257.0011 [log in to unmask] http://www.vtcircuits.com -----Original Message----- From: Kristopher J. Keating [mailto:[log in to unmask]] Sent: Tuesday, April 06, 2004 2:18 PM To: [log in to unmask] Subject: Re: [TN] SNEC Mtg Hello, Is there an IPC spec or some other industry standard for "surface bites" or "dish downs"? How big of a "bite" is acceptable? Kristopher J. Keating --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------