SenJoon 2 Reasons are possible for this kind of failure 1) Popcorning: Delamination of the molding from the chip ripping off the bonds 2) bad soldering Solutions: 1) Dry all BGAs before soldering, keep temperature as low as possible, control heat up rate. 2) Difficult to say, need first to find out why the beggars don't solder. --> Reason 1 is quite common. Best regards Guenter EMPA Swiss Federal Laboratories for Materials Testing and Research Centre for Reliability Guenter Grossmann, Senior Engineer 8600 Duebendorf Switzerland Phone: xx41 1 823 4279 Fax : xx41 1 823 4054 mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------