The Scanpoint from diagnosys is a quick inline machine. From my experience, it will check 1200 parts for presence in under 2 minutes. Mark ===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at 29/04/04 14:08 >I wish I made myself clear. We have a very high volume low-mix environment >here. We are looking for inline units only. >Rama > >---------- Forwarded Message ---------- > > >Hi, >If you want to check for the presence or absence of some transparent-to-test >components only, I'd like to introduce benchtop AOI machine, there are many >makers, such as: Marantz, Mirtec, Saki, Scanpoint... >The price is around 30K USD. >Bye. >**************************************************************************** >****** >TRAN TIEN PHAT >MANAGER, PCBA MANUFACTURING DEPARTMENT. >FUJITSU COMPUTER PRODUCTS OF VIETNAM, Inc. >No. 31, 3A street, BIENHOA INDUSTRIAL ZONE #2, DONGNAI province, VIETNAM. >Tel: 84-61-836563 ~ 66. >Fax: 84-61-836561 ~ 62. >H/P: 84-903908385 >Email: [log in to unmask] >**************************************************************************** >*** >----- Original Message ----- >From: "Rama Vemulapalli" <[log in to unmask]> >To: <[log in to unmask]> >Sent: Thursday, April 29, 2004 6:13 AM >Subject: [TN] AOI > > >> We have decided to purchase AOI equipment to check for the presence or >absence of some transparent-to-test (Incircuit test) components. Would any >of you ( who use AOI in your plants) give me some feedback about the systems >available in marketplace ? >> >> Thanks >> Rama Vemulapalli > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-509-9700 ext.5315 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------