Morning Jeffrey, Not sure if this fits your scenario, but...... We're a prototype bare board shop. One of our customers specifies red soldermask for engineering proto's & green mask for production runs. Another customer specifies yellow ink marking along the board edge for engineerng proto orders. Regards, Mark -----Original Message----- From: McGlaughlin, Jeffrey A [SMTP:[log in to unmask]] Sent: Tuesday, April 13, 2004 10:39 AM To: [log in to unmask] Subject: [TN] Prototype Identification I am looking for a "best practice" for identifying engineering prototype boards in a high-mix low-volume production environment. In the past we have been a prototype only facility but are adding the capability to do small run production in house. Since we have more engineers than production techs we often have engineers involved with assembly and need to track their project development boards separately. TIA, Jeffrey A McGlaughlin, CID Engineering Designer Battelle Memorial Institute Columbus Ohio http://www.battelle.org [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------