I would echo that sentiment. In my brief experience with ENIG (and black pad), it seems to come when there are already smaller/less significant problems with the ENIG plating or other processes (i.e. everything pretty much goes south at the same time...:) -----Original Message----- From: Jana Carraway [mailto:[log in to unmask]] Sent: Monday, April 05, 2004 11:54 AM To: [log in to unmask] Subject: Re: [TN] Black Pad Prevalence Importance: Low I'm not an expert in ENIG, but having spent 20+ years in this industry, experience tells me that the success, or lack thereof, of any process is directly related to the company and people running the process. I do not think ENIG is much different from my experiences installing, running, and troubleshooting imaging processes; whether it is DuPont, Dynachem (past history), or Hitachi (more current history), each resist has positives and negatives, distinct process windows, and the success is more often dependent on the ability of a facility to optimize for the product or technology. The key to the successful operation of any process is understanding the variables and controlling those variables for optimum process and product performance. I am uncomfortable with generalizations comdemning any given technology, particularly one that is as widely used as ENIG. I know there are companies successfully producing and utilizing ENIG surfaces. We have used it for over 4 years with very, very few issues and no line down situations due to the surface finish or black pad. I suspect that, as an industry, we have not learned all the critical variables or interactions with ENIG, thus, we have not fully optimized the process. Just my opinion, Jana Carraway Lake Oswego, Oregon -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Jeffrey Bush Sent: Monday, March 29, 2004 5:15 AM To: [log in to unmask] Subject: Re: [TN] Black Pad Prevalence ENIG processes are costly to maintain and this finish if not the preferred solution for soldering planarity. The Nickel deposition process requires a good deal of attention and the main issue is the process going south is the lack of work being processed through it. The cost of ownership of the ENIG outweighs the benefits sharply and both tin and silver exist as economic alternatives to gold and do not have the disadvantages which go beyond the black pad condition. Silver appears to be the most effective alternative as it is more forgiving for time delays between thermal excursions, but many assemblers have adapted their process to also run tin effectively, which has the lowest overall cost impact per unit. Stay away from ENIG and evaluate tin and/or silver. Jeffrey Bush Director, Quality Assurance and Technical Support 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302-1890 Tel. 802.257.4571.21 Fax. 802.257.0011 [log in to unmask] http://www.vtcircuits.com -----Original Message----- From: Paul Truit [mailto:[log in to unmask]] Sent: Saturday, March 27, 2004 10:03 AM To: [log in to unmask] Subject: [TN] Black Pad Prevalence I have searched the archives and have found lot's of good info but nothing in regard to the prevalence or the statistical occurrences of this event. I have run tens of thousands of ENIG boards and I haven't observed this defect but I am concerned enough to ask. Is this a board fabricator controllable issue that has been minimized? Have you observed this phenomenon? How often will this occur? Is immersion silver the better way to go to assure the reliability and quality of the products? -- Paul Truit, Mfg. Eng. RBB Systems, Inc. 4265C E. Lincolnway Wooster, OH 44691 Ph. (330) 567-2906 ext 514 Fax (330) 263-5324 Email: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------