IMHO, not a good idea to tin wire wrap "spikes". The sharp corner should penetrate the wire slightly to provide an intimate interface that cannot oxidise. The one time I had a job like that, we used preforms on each spike and reflowed in an IR oven. The stamped preforms were in the form of strips of "washers" at 0.156" pitch with the stem between each washer fairly thin. We had to apply the flux to the board before threading the preforms. We made them ourselves using solid solder strip as the starting point. If I had to do it today, I think I'd dispense a blob of solder paste (it didn't exist in the late 60s) with an X-Y-Z dispenser. Fortunately, we had only about a dozen to make, but each one had over 10,000 spikes from the back of connectors. The only "wiring" on the single-sided 2.4 mm PCB was the power connections (I think ±15 V for analogue and +5 V for digital plus the two grounds). All the signal wiring was wire-wrapped. Brian Steve Gregory wrote: > Mornin' All! > > One of the guys from our bid department asked me to come and look at a > backplane we're bidding on, and tell him how we would solder it? I went and looked > at it, and I'm not sure how we would. Go to http://www.stevezeva.homestead.com > and take a look at Backplane Topside, Backplane Backside, and Backplane > Backside Leads. > > The leads for all the connectors protrude at least a half inch or longer out > the bottom of the board. I'm assuming they are that long because they get wire > wrapped after the backplane is assembled. But how do you solder something > like that? Some sort of dip solder pot? Drag solder? I don't think I'm going to > be able to solder a board with leads that long in our Electra wave solder. > > I can tell board was mass soldered, and I'm thinking it was dipped somehow. > Because you can see tiny little peaks on most of the lead tips that go straight > up and down. Is there such thing as some sort of dip solder machine? > > Sorry for all the dumb questions, but I've never been around a backplane like > this, and don't really know how something like this gets built. > > Thanks! > > -Steve Gregory- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > ----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------