Hi Ioan, You automotive environment is the harshest [short of down-hole drilling] for electronic assembliies--just look at the millions of SUVs GM has to recall because of solder joint failures. In a harsh environment, any voids in via solder fill creates stress risers and thus reduce reliability. What would work for many years in a telecom environment would fail quickly in an automotive under-hood environment. The life ratio for unfilled vias is about a factor of 1000. Thus, in your environment I would not allow any voids in solder-filled vias; voids in polymeric fills of vias are not very important. And, as Robert pointed out, solder joint reliability degradation mmay be even more important. Regards, Werner Engelmaier Engelmaier Associates, L.C. Electronic Packaging, Interconnection and Reliability Consulting 7 Jasmine Run Ormond Beach, FL 32174 USA Phone: 386-437-8747, Fax: 386-437-8737 E-mail: [log in to unmask], Website: www.engelmaier.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------