One thing to know is that AR can be coated to patch UR but not the other way around. Patching AR with UR creates a mix that takes too long to dry, stays soft. So to switch from UR to AR is recommended. Regards, Ramon > -----Original Message----- > From: - Bogert [SMTP:[log in to unmask]] > Sent: Monday, March 08, 2004 4:55 PM > To: [log in to unmask] > Subject: [TN] Pros and Cons on Type UR vice Type AR Conformal Coating > > As a Class 3 customer we are considering mandating transition from Type UR to Type AR conformal coating, to make it easier to replace failed components. Are there any Class 3 users of Type AR coating? What is track record for using Type AR? Are there any compatibility issues with certain types of solder masks? Any input you have would help. Another advantage with AR would be for returned equipment. The OEM could remove all the coating from an assembly using alcohol, then perform > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > ----------------------------------------------------- > bed-of-nails testing to quickly identify failed components. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------