Just a note here. If the hole is not supported, it's defect, be careful with that. Also, note 2 on page 5-16 points out: "For plated-throuh hole boards greater than 2.3mm thick, components with pre-establish lead lenghts, (DIPs, Sockets), lead protrusion may not be discernible." Personnally, in such a case I would also make sure that soldering on primary side meets 270deg wetting on lead. My two cents... JF -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Lance Mayes Sent: Thursday, March 04, 2004 4:34 PM To: [log in to unmask] Subject: [TN] Lead Protrusion Importance: High TechNetters: I have a question on lead protrusion. We have ordered in components that does not come through the PCB like it states in IPC-A-610C, 5.2.7.1, figure 5-34. It is more along the L Min in the figure 5-34. Is this acceptable for Class 2 manufacturing? I told my supervisor this is a process indicator and should be corrected but he wants some more input and so do I before we give the go ahead. Anxiously waiting. Thanks P. Lance Mayes --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- Mfg. Trainer ***** CONFIDENTIALITY NOTE ***** The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------