Dear Soldering Gurus, I currently have a dewetting problem with silver electroplated parts and I was hoping that Technet would provide me with some suggestions. A brief history - Our silver plating solution has been changed as our old solution is no longer available. We are using water soluble 62/36/2Ag solder paste. Our soldering process works very well on old tarnished components from the previous plating solution, but demonstrates dewetting in components plated with the new solution. The rest of the process appears to be the same. Any hints on particulars to watch out for or test would be greatly appreciated. Regards and thanks, Jeff Brown The Australian National University --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------