The article Steve mentions doesn't address existing equipment that has been in use. I want to know how successful would it be to disassemble the wave and it's components that come in contact with the solder and have them reworked with Melonite. I was also wondering if someone has done so, how much did it cost and was it effective. Scott. -----Original Message----- From: Steve Gregory [mailto:[log in to unmask]] Sent: Wednesday, February 04, 2004 2:21 PM Subject: Re: Solder Bath Coating "Melonite" Hi Scott! There was a good paper presented at last years Apex that talked about Melonite treated stainless called "Equipment Impacts of Lead Free Wave Soldering". The article is up on the web, just do a Google search of the title and you'll find it... it's pretty good. The article was recognized as the best paper presented at Apex 2003, and explains all the tests that were done on different materials. Melonite coating is more of a process of treating the steel than anything else, and it does provide more protection. But if the Melonite/Nitrided steel becomes scratched, it will degrade. The protection from Melonite is also dependant on the type of stainless steel the parts are made from, 304 stainless is better than 316 stainless. Even then, inspections should be done every 6-months for the 304, and every 3-months for the 316. -Steve Gregory- > I understand, the wave solder manufactures are treating their solder bath > and components with melonite so it will be compatible with Pb free solders. I > have found a company that will coat our older wave solder components with > melonite. Has anyone done such a thing, how much did it cost and was it > successful? > > Thanks > > Scott > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------