Hi Guenter! Yes, there are a number of property differences between electrolytic and galvanic nickel - characteristics such as elongation, hardness, corrosion resistance, etc., which a design can use to his/her advantage during designs. Dave Hillman Rockwell Collins [log in to unmask] Guenter Grossmann <Guenter.Grossman To: [log in to unmask] [log in to unmask]> cc: Sent by: TechNet Subject: [TN] Ni galvanic / chemical <[log in to unmask]> 02/05/2004 02:01 AM Please respond to "TechNet E-Mail Forum."; Please respond to Guenter Grossmann Hi all Are there any differences in the properties of the plating when an Ni plating is chemically deposited or with a galvanic process? Best regards Günter EMPA Swiss Federal Laboratories for Materials Testing and Research Centre for Reliability Guenter Grossmann, Senior Engineer 8600 Duebendorf Switzerland Phone: xx41 1 823 4279 Fax : xx41 1 823 4054 mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------