Yes -- If you are upgrading equipment for Pb Free, definitely have the option for Nitrogen added to the equipment. IF you choose NOT to use the nitrogen, you can do so through the recipe. It will be easier NOT to use Nitrogen when you are plumbed for it than to Try to use Nitrogen when you are NOT plumbed for it. -Carrie -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Scott Lefebvre Sent: Friday, February 27, 2004 1:26 PM To: [log in to unmask] Subject: [TN] Use Nitrogen or Not! I am looking at upgrading our Reflow and Wave Solder equipment for Pb free. I wanted to know what the consensus is for the requirement of Nitrogen for these two systems. It seems to depend on who you ask some say you will need Nitrogen and others say no. Thanks, Scott Lefebvre --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------