You can try "Steel Red Dye" from Dykem. You can find it here. http://www.dykem.com/Products/MarkingSystems/LayoutFluids/steelred.htm The sell a thinner for the dye as well. Vladimir Igoshev, Research in Motion 451 Phillip St. Waterloo, ON, N2L 3X2 Voice: (+1) 519-888-7465, ext. 5283 Fax: (+1) 519-886-0863 E-mail: [log in to unmask] <mailto:[log in to unmask]> -----Original Message----- From: Stolar, Paul W [mailto:[log in to unmask]] Sent: Tuesday, February 17, 2004 4:36 PM To: [log in to unmask] Subject: [TN] Dye Does anyone have experience with dye penetrant on assembled PC boards? Questions are: 1. any special dye? 2. how to clean? Paul Stolar Materials/Reliability Engineer Manufacturing Reliability Lead Engineer Baker Atlas 713-625-5376 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------