Guenter Most decidely. The crystalline structure, to start with. As chemical plating is a replacement method, it tends to take a similar structure, in its very thin layer, to the substrate metal whereas electrolytic metals tend to form their own structure, which is, more often than not, governed by the additives in the plating solution. Chemically, both are likely to have non-metallic co-deposits, but they will be entirely different. Brian Guenter Grossmann wrote: > Hi all > > Are there any differences in the properties of the plating when an Ni plating is chemically deposited or with a galvanic process? > > Best regards > > Günter > > EMPA > Swiss Federal Laboratories for Materials Testing and Research > Centre for Reliability > Guenter Grossmann, Senior Engineer > > 8600 Duebendorf > Switzerland > > Phone: xx41 1 823 4279 > Fax : xx41 1 823 4054 > mail: [log in to unmask] > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > ----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------