I do not see why you can not just use the boards as is. Trying to rework boards and putting them again through HASL will only increase the possibilities for trouble. The gold plated areas will be covered with solder when you put them through you wave so you are basically doing in house what you board supplier is trying to do during rework. Scott Westheimer ----- Original Message ----- From: "Ezequiel Cruz" <[log in to unmask]> To: <[log in to unmask]> Sent: Wednesday, February 04, 2004 9:47 AM Subject: [TN] Rework Gold Finish > Can anyone help with the following: > > My board house built my boards with a gold finish. > The finish should have been selective gold as we have some contact areas on > the pwb. > > I have insisted on a re-build which is currently being done. However, > because of our all ready late schedule, the board house has offered to re- > work the gold finish boards for us. The method explained to me was mask the > selective gold areas and flux clean the remaining board while dipping in > molten solder. > > Does anyone have any experience with re-working this way. Our biggest > concern is from a re-liability standpoint. Obviously this board will go > through additional thermal cycling not necessarily part of a standard > build. What effect, if any, will this have on the board itself. Remember > that our stuffing house will place this board through additional thermal > cycling. > > Any help is greatly appreciated. > > Ezequiel Cruz > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------