(chuckling at all this) First of all, I did ask questions in my initial response, they are pasted below ((Where are you seeing this at? over ground planes? on traces? glass? are you seeing it before processing? (bare boards) are they using LPI or UV mask? what color? do you observe contamination os discoloration in the area after the mask has flaked off?)) From the asking of these questions one could safely assume I am attempting to isolate a specific 'process' variable that would cause flaking mask...a fabrication process... From Scott's response, it appeared to be right out of the gate a "fab issue" which is not always the case...too many times it is a "fab issue" (as determined by assemblers) and the root cause not actually found...too often most assembly issues become fab issues thus not focusing in on root assembly causes. I was attempting to bring additional comments and perspectives into the conversation in line with the intent of TechNet... I've not seen any pictures as of yet so I cannot offer any information, as far as I know no one else has either...and while I certainly realize that most, most, thats most causes of flaking mask are the result of actions or inaction on the part of the fabricator, is it in everyones best interest to assume this is the case here? Okay, enough rambling, got fabrication matters to address...(grin) Franklin --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------