Doesn't sound like a good idea to me. I'm sure that adhesion will be a BIG problem. RTV, apart from being a silicone, cures on the outside skin first, working down to the middle of the "blob". The polymerisation is a condensation reaction, working on humidity being drawn into it. This can take weeks or months before it is complete. It won't stop because of the coating, just slowed down, so you will be pumping humidity through your coating for a long time, just at a place where little or no bonding can occur between the coating and what is under it. Get the picture? I appreciate the need to fix the components, but why RTV? If you use a correctly mixed and cured epoxy, you will have no problems. I must admit that I'm "allergic" to silicones of any nature being used for anything in electronics, where they can be avoided. They are never a good protection and they are generally quite fragile. Their only usefulness, IMHO, is for high-temperature insulation, provided they are supported with, e.g., glass fibres. Brian Mark Charlton wrote: > My learned and esteemed colleagues, > > One of our customers has requested that we conformal coat over a DOW 3145 > RTV adhesive used to stake some sensitive components. The specified coating > material is MS470-N, a urethane product. > > Is this a standard practice (to coat over RTV)? We have always conformal > coated the PCA and then staked the components using the RTV. Our CC vendor > isn't too pleased with this request. > > Mark Charlton > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > ----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------