Robert Sefton wrote: > > snip < > But some of the other reasons listed here also > seem plausible. Hi Robert, In fact many are saying the same thing you postulate in varying degrees of clarity. Primary factors as I understand things are the fab plate and etch process control as well as (I think it was Bell- core) minimizing unncessary copper removal. Have seen thieving added on inner layers in an effort to help bow and twist and have heard the assembly "uniform heating" before, although it strikes me that was in the early days of reflow. The wave-solder comment is the same word used in different context. For some closely-spaced parts (ie 050 pitch SOIC and perhaps 2mm through-hole connectors) adding a sacrifi- cial pad is used as a pre-emptive measure expecting the last two pads drawn out of the solder to bridge. Usually the electrical impacts of note regards proximity to same-layer traces, presence of traces on a layer adja- cent to theiving, and reduction of regulatory spacings not obvious to a fabricator. -- Jeff Seeger Applied CAD Knowledge Inc Chief Technical Officer Tyngsboro, MA 01879 jseeger "at" appliedcad "dot" com 978 649 9800 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------