Ezequiel, I have seen very good success with that rework method. If they do it right, you will not be able to tell the difference. If the masking doesn't hold, you might get some wisps of solder on the contact pads, but the integrity of the gold will remain. Save yourself and the board house some grief. Accept the reworked boards. DOug On Thu, 5 Feb 2004 08:36:00 +0200, Reuven ROKAH <[log in to unmask]> wrote: >You should take care to the cleanliness of the PCBs after the process. >If the PCBs have plugging via holes, active residues can be left there and >it almost impossible to remove them. >Also solder balls from the HASL process can be created in via holes. > >The good things are that the PCBs have new finish (solderability) and 100% >thermal stress. > > >Best Regards > >ROKAH > > > > Eddie Rocha > <[log in to unmask] To: [log in to unmask] > om> cc: > Sent by: TechNet Subject: Re: [TN] Rework Gold Finish > <[log in to unmask] > > > > > 04/02/2004 19:48 > Please respond > to EddieR > > > > > >If the amount of gold is less than ~20 uin, then rework might be an >option. Too much gold will result in embrittlement issues with your >solder joints. > >On 4 Feb 2004 at 8:47, Ezequiel Cruz wrote: > >Can anyone help with the following: > >My board house built my boards with a gold finish. >The finish should have been selective gold as we have some >contact areas on >the pwb. > >I have insisted on a re-build which is currently being done. However, >because of our all ready late schedule, the board house has offered >to re- >work the gold finish boards for us. The method explained to me was >mask the >selective gold areas and flux clean the remaining board while >dipping in >molten solder. > >Does anyone have any experience with re-working this way. Our >biggest >concern is from a re-liability standpoint. Obviously this board will go >through additional thermal cycling not necessarily part of a standard >build. What effect, if any, will this have on the board itself. >Remember >that our stuffing house will place this board through additional >thermal >cycling. > >Any help is greatly appreciated. > >Ezequiel Cruz > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV >1.8e >To unsubscribe, send a message to [log in to unmask] with >following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: >http://listserv.ipc.org/archives >Please visit IPC web site >http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional >information, or contact Keach Sasamori at [log in to unmask] or 847- >509-9700 ext.5315 >----------------------------------------------------- >-- Thanks, >Eddie Rocha >(408) 978-8992 x 282 > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-509-9700 ext.5315 >----------------------------------------------------- > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------