IPC TM-650 Test Methods Manual 2.3.38B Surface Organic Contaminant Detection Test - 8/97 Involves Methyl Cyanide so recommend use a laboratory.... -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Richard Kraszewski Sent: Monday, January 12, 2004 1:26 PM To: [log in to unmask] Subject: [TN] J-Stnd-001 Section 8.31 (Particulate Matter) I'm seeking input on how organizations confirm that they meet the requirements of J-Stnd-001, section 3.1 for particulate matter? I image that one could collect a sample (somehow?) and inspect under magnification, but I'm looking for specific methods & their details. It sure would be nice to identify a method that would actually have a chance of passing an MSE. Any thoughts? Rich Kraszewski Advanced Manufacturing Engineer - KEDS 1038 E. 15th Street, Jasper, IN 47546 Phone: 812.634.4281 Pager: 812.481.3492 E-mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------