Put it this way, Steve. Karl Dietz published his book "Dry Film Photoresist Processing Technology" in 2001, with its sexy pink dustcover. In the 430-odd pages, there are a few mentions of solder masking in Chapter 1 with a solid implication that it has been supplanted entirely by LPI. Dr Dietz is pretty high up in the company that introduced dry film technology, including solder masks, to the world. Need one say more? Brian Steve Gregory wrote: > Can anybody tell me why dry film solder masks are still specified? > > I don't want to hear; "Because they've always worked good..." > > But some clear, concise, reasons for specifying them... > > Vacuum at ICT is a dead deal, there are ways to deal with open via's with > LPI's...Solder fill for via's is a dead deal...either you fill them, or you don't. > > So why dry-films? > > So many complications come up with dry film solder masks... > > Not only for the bare board manufacturer...but also for the assembler. > > Just a question...(for the DoD guys, especially) > > -Steve Gregory- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > ----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------