Yes, kapton supplies are very tight. The major offshore manufacturers are quoting lead times of 12-20 weeks. On shore DuPont is better but still running 2-5 weeks depending on the material construction. Some offshore capacity will come on line about mid-2004 but the rumour is that it is already sold out. Other major capacity will not come on line until 2005. There is really no alternative to kapton or its' derivatives especially in rigid flex. In addition most good flex shops are very busy. Good luck. Regards Steve Kelly -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack C. Olson Sent: Wednesday, January 07, 2004 12:48 PM To: [log in to unmask] Subject: [TN] Bare Board Fab: Flex Material Shortage? I have a question for the bare board manufacturers out there, is there a shortage of polyimide these days? I don't usually have much to do with material, but we are having trouble getting rigid-flex quotes for less than 14 weeks out. Is there an alternative to kapton? Are any vendors known for fast-turn rigid flex? suddenly behind schedule, Jack --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------