You need to add humidifiers to increase the humidity. Worked in a clean room with 30%RH and yes it can be very uncomfortable and with the dryer air hugh amounts of Static is generated. You can use either portable Humidifiers or have it controlled into your central air system. Immediate relief is portable units. May even try a vaporizer (mom my nose is stuffy) for local areas if needed. Randy Bock Sr. Quality Manager GMS Naugatuck (p) 203 720-3861 (f) 203 729-5397 (email) [log in to unmask] "Sergio T. Ruiz" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 01/06/2004 10:25 AM Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to "Sergio T. Ruiz" <[log in to unmask]> To [log in to unmask] cc Subject [TN] etest environment.. after trying a few different methods to control our environment for our etest room (the one i am referring holds only our everett charles 9090) system, we are finding that the room is very uncomfortable.. as soon as winter hit, and the humidity started to plummet, we added a humidifier to the room.. according to spec, we are keeping it in the 45% range. we are finding that in order to keep it there, we are having to keep the temperature in the 72F range.. the impetus for examining this more was losing a few cards to static electricity.. this is a big bucks problem, and we needed to get it solved immediately.. can anyone else tell me if they have experienced such an uncomfortable environment? thanks! ____ Sergio T. Ruiz technology and MIS Philway Products, Inc. (419) 281-7777 x232 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------