Ioan, A lot of this will depend on the type of product you are manufacturing. If you are producing a product like a PDA, you will be able to get by with a 235-245 C peak temp. If you are building bigger boards with heat sinks, etc. you may have to go to 260C (good luck!). Being in the lucky group we are not going to have to change our boards at all. We are now squeezing the component suppliers to get components that can meet the temp profile requirements. You need to engage your designers NOW so they pick appropriate components for new designs so you don't have to go through the whole process again. Ammo? If they don't help you and you don't get parts, you won't be able to sell into Europe. Period. Bev Christian Research in Motion -----Original Message----- From: Tempea, Ioan [mailto:[log in to unmask]] Sent: November 6, 2003 9:33 AM To: [log in to unmask] Subject: [TN] Lead free and product design Hi Technos, "our designs are perfect, lead-free is a manufacturing problem"... Does this sound familiar to you? Well, I got to hit this wall, me too. Our product developpers don't really feel like they should hop into this train. There are 2 things I would like to ask you: * what ammo (technical, of course) should I use to change their minds * besides deciding on a suitable alternative finish of the PCB, higher Tg FR4, picking the right components, is the intimate design of the PCBs affected by the Pb-free? I mean, different land patterns, clearances, via technologies, etc.? What about solder masks and marking inks? Any clue would be largely appreciated. Thanks, Ioan --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------